Reminder to CLC members, please make sure that your CLC number is stored in the relevant field in your forum profile. This is important for the upcoming change to the Forums access, More information can be found at the top of the General Discussion forum. To view or edit your profile details, click on your username, at the top of any forum page. Your username only appears when you are signed in.

Main Menu

Freeze Plug Diameter

Started by pauldridge, September 27, 2012, 08:34:33 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Tom Beaver

In the past the foundry used to in-bed wire in the sand molds to act as reinforcing bars.  After casting the block they would flush the sand out of the block cavity and usually removed the wire also, but not always.  I have seen this a time or two.  This is most likely what you see and you can just remove it and throw it away.

Tom Beaver

sjocad

I found it.
It was an old velding rod" there.May be lost when they took the dirt out.Now its ok.
Thanks folks... :-[
svein sjoblom,CLC # 12214.